From the perspective of the wigs manufacturer, Answer some human hair products questions.

From the perspective of the wigs manufacturer, answer some human hair products questions. Include the maintenance, washing, manufacture, fading, shedding an so on, we will update some topic base on customer question every month.

Which kinds wigs is more durable? Which kinds wigs is more good value for money? Why the wigs fading color? How to maintain the wigs?

Which kinds hair is best hair? Which kinds hair is complex for manufacture? How to check real human hair?

Why does other people wear 1 year, but I only wear 6 months?

Where is the real human hair base in China, why they use the north Korea workers?

how to buy the good quality wigs, how to avoid being duped?

how to distinguish the wigs?

……

Today we talk the hair of Wig fading color, Human hair quality changes, washing and care problems.

Let’s talk about the composition of hair color. The hair is divided into three sections: the epidermis (hair cuticle), the cortex (pigment is in here), and the medulla (think of the center of the tree, the core).

Natural human virgin hair(cut from the girl directly), unprocessed virgin human remy hair, virgin human hair (excluding dyed and perm hair)

All the original natural black hair, the primary pigment has composed of red, yellow and blue. 1.Blue pigment is the most, but blue color fastness is relatively weak. 2.Yellow pigment is the least, but the color fastness is strongest. 3.Red pigment is centered.

If you’d bleached the hair, you should know the color will be fading when the bleaching agents on the hair, it doesn’t add the pigment to your hair. Blue pigment removes, the color is change from black to red (brown), when red pigment removes, the color is change to yellow. Usually the #613 and #60 is the lightest bleach color. We’re talking about bleach process, it is process of fading.

What about regular hair coloring, it is not like paint to cover the hair surface.
Conventional hair dyeing is to use hydrogen peroxide milk to open up the first layer of hair cuticle. Remove the pigments corresponding to the degree of hydrogen peroxide emulsion, then bring the artificial pigments into the second layer of cortex, and combine with the natural pigments, so that we can present the color we want to dye.

What about regular hair coloring, it is not like paint to cover the hair surface.
Conventional hair dyeing is to use hydrogen peroxide milk to open up the first layer of hair cuticle. Remove the pigments corresponding to the degree of hydrogen peroxide emulsion, then bring the artificial pigments into the second layer of cortex, and combine with the natural pigments, so that we can present the color we want to dye.

So why does it fade?

Because the color fastness of blue pigment is relatively weak.
The hair cuticle will open when the hair encounter alkali and heated, the blue pigments will be lost gradually. The degree of fading depends on the hair quality. Of course, the dyed dark hair is relatively slower. Because it added a lot of dark pigment in to the hair, the natural hair has no dark pigment.
Most middle-end to high-end hair products require deacidification to remove the hair cuticle. If washing with alkaline shampoo, the pigment will accelerate loss.

So the solution of the fading problem is to use low alkalinity shampoo, and use relatively high silicone oil content shampoo, and then use the hair conditioner.The cleaning frequency is 10 to 15 days. If the loss of pigments is serious, go back to the factory or go to the hairdresser. Pay attention here, do not use dandruff, oil control, cool mint and other types of shampoo, it is better to use wig special shampoo, conditioner. Professional washing and protecting products are related to the ratio of deacidification liquid and ph.

Indian hair relatively is less blue pigment, fading will be faster, of course, because the Indian hair is not good, if the hair faded serious and can not be used. Just change a new one…

Hair quality change,  most customers understand that the natural virgin hair is the best hair quality in the hair industry, down is the virgin remy hair, virgin hair. Let’s take natural virgin hair for example.

After deacidification, the flexibility and plasticity of hair quality are also excellent. However, due to the daily washing and care products, ultraviolet radiation, sweat, swimming pool water, sea water and other external factors, hair quality are changing in the daily.

Who wants to tell you that his hair is the same for life, then please stay away from him. J
Basically, the flexibility, agility and plasticity of virgin braids are no problem for 1-2 years even if the hair cuticle are removed. However, due to inappropriate daily care, hair quality will deteriorate faster.

So we need to pay attention to the following points. 1.Refer to the above fading coping methods, 2.Daily care , do not rub, natural air drying (if use hair dryer, do not use hot air), 3.Reduce or aviod the swimming pool, sea water. 4.If sleeping with a wig, put a scarf or silk on your pillow.

The best state of wigs is the state of the end of care,  It’s impossible to achieve the effect of star styling without taking care of it. But remember, hair styling appliances (rollers, splints, etc.) are suitable for 130-150 degrees Celsius.

For the problem of shampoo and care, there are special techniques and skills, remember not to rub. Major use of patting, pinching, grabbing, etc. If you don’t understand, feel free to contact us. www.fsnwigs.com  